1. The feeding environment is sealed as far as possible, so that it is not easy to fall into large particles with the air flow.
2. rotten packaging silicon carbide powder should not be used as far as possible, after rotten packaging may have been mixed with impurities, affecting the cutting effect.
3. In the use of slurry, tools should be controlled to prevent cross-use pollution.
4. Spare feeding slurry should be stored for a long time. If it is too long, it will produce cohesion and form fake particles, which may affect wire cutting.